Effect of thermal annealing on dielectric and ferroelectric properties of aerosol-deposited $0.65\text{Pb}(\text{Mg}_{1/3}\text{Nb}_{2/3})\text{O}_{3}-0.35\text{PbTiO}_{3}$ thick films

Fuente: arXiv
Enregistré dans:
Détails bibliographiques
Auteurs principaux: Nadaud, Kevin, Sadl, Matej, Bah, Micka, Levassort, Franck, Ursic, Hana
Format: Preprint
Publié: 2023
Sujets:
Accès en ligne:
Tags: Ajouter un tag
Pas de tags, Soyez le premier à ajouter un tag!
_version_ 1866914831514206208
author Nadaud, Kevin
Sadl, Matej
Bah, Micka
Levassort, Franck
Ursic, Hana
author_facet Nadaud, Kevin
Sadl, Matej
Bah, Micka
Levassort, Franck
Ursic, Hana
contents In this work, the effects of thermal annealing at 500 °C on aerosol-deposited $0.65\text{Pb}(\text{Mg}_{1/3}\text{Nb}_{2/3})\text{O}_{3}-0.35\text{PbTiO}_{3}$ thick films on stainless-steel substrates are investigated using two complementary methods at high and low applied external electric fields. The first one is Positive Up Negative Down method, which allows us to obtain information about the switching and non-switching contributions to the polarization. It shows that the as-deposited film is ferroelectric before annealing, since it has a switching contribution to the polarization. After annealing, both the switching and non-switching contributions to polarization increased by a factor of 1.6 and 2.33, respectively, indicating stronger ferroelectric behavior. The second method is based on impedance spectroscopy coupled with Rayleigh analysis. The results show that post-deposition thermal annealing increases the reversible domain wall contribution to the dielectric permittivity by a factor 11 while keeping the threshold field similar. This indicates, after annealing, domain wall density is larger while domain wall mobility remains similar. These two complementary characterization methods show that annealing increases the ferroelectric behavior of the thick film by increasing the domain wall density and its influence is visible both on polarization versus electric field loop and dielectric permittivity.
format Preprint
id arxiv_https___arxiv_org_abs_2310_18005
institution arXiv
publishDate 2023
record_format arxiv
spellingShingle Effect of thermal annealing on dielectric and ferroelectric properties of aerosol-deposited $0.65\text{Pb}(\text{Mg}_{1/3}\text{Nb}_{2/3})\text{O}_{3}-0.35\text{PbTiO}_{3}$ thick films
Nadaud, Kevin
Sadl, Matej
Bah, Micka
Levassort, Franck
Ursic, Hana
Materials Science
In this work, the effects of thermal annealing at 500 °C on aerosol-deposited $0.65\text{Pb}(\text{Mg}_{1/3}\text{Nb}_{2/3})\text{O}_{3}-0.35\text{PbTiO}_{3}$ thick films on stainless-steel substrates are investigated using two complementary methods at high and low applied external electric fields. The first one is Positive Up Negative Down method, which allows us to obtain information about the switching and non-switching contributions to the polarization. It shows that the as-deposited film is ferroelectric before annealing, since it has a switching contribution to the polarization. After annealing, both the switching and non-switching contributions to polarization increased by a factor of 1.6 and 2.33, respectively, indicating stronger ferroelectric behavior. The second method is based on impedance spectroscopy coupled with Rayleigh analysis. The results show that post-deposition thermal annealing increases the reversible domain wall contribution to the dielectric permittivity by a factor 11 while keeping the threshold field similar. This indicates, after annealing, domain wall density is larger while domain wall mobility remains similar. These two complementary characterization methods show that annealing increases the ferroelectric behavior of the thick film by increasing the domain wall density and its influence is visible both on polarization versus electric field loop and dielectric permittivity.
title Effect of thermal annealing on dielectric and ferroelectric properties of aerosol-deposited $0.65\text{Pb}(\text{Mg}_{1/3}\text{Nb}_{2/3})\text{O}_{3}-0.35\text{PbTiO}_{3}$ thick films
topic Materials Science
url https://arxiv.org/abs/2310.18005