Controlling ultrafast laser writing in silica glass by pulse temporal contrast

Fuente: arXiv
Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Lei, Yuhao, Wang, Huijun, Shayeganrad, Gholamreza, Svirko, Yuri, Kazansky, Peter G.
Format: Preprint
Veröffentlicht: 2024
Schlagworte:
Online-Zugang:
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
_version_ 1866929212964732928
author Lei, Yuhao
Wang, Huijun
Shayeganrad, Gholamreza
Svirko, Yuri
Kazansky, Peter G.
author_facet Lei, Yuhao
Wang, Huijun
Shayeganrad, Gholamreza
Svirko, Yuri
Kazansky, Peter G.
contents Control of laser writing in transparent dielectrics using temporal contrast of light pulses is demonstrated. Anisotropic nanopores in silica glass are produced by high-contrast of 10^7 femtosecond Yb: KGW laser pulses rather than low-contrast of 10^3 Yb fiber laser pulses. Low-contrast pulses are useful for creating lamellar birefringent structures, possibly driven by quadrupole nonlinear current. The difference originates in the fiber laser storing third of its energy in a post-pulse of 200 ps duration. The absorption of this low-intensity fraction of the pulse by laser-induced transient defects with relatively long lifetime and low excitation energy, such as self-trapped holes, drastically changes the kinetics of energy deposition and type of material modification.
format Preprint
id arxiv_https___arxiv_org_abs_2401_09055
institution arXiv
publishDate 2024
record_format arxiv
spellingShingle Controlling ultrafast laser writing in silica glass by pulse temporal contrast
Lei, Yuhao
Wang, Huijun
Shayeganrad, Gholamreza
Svirko, Yuri
Kazansky, Peter G.
Optics
Applied Physics
Control of laser writing in transparent dielectrics using temporal contrast of light pulses is demonstrated. Anisotropic nanopores in silica glass are produced by high-contrast of 10^7 femtosecond Yb: KGW laser pulses rather than low-contrast of 10^3 Yb fiber laser pulses. Low-contrast pulses are useful for creating lamellar birefringent structures, possibly driven by quadrupole nonlinear current. The difference originates in the fiber laser storing third of its energy in a post-pulse of 200 ps duration. The absorption of this low-intensity fraction of the pulse by laser-induced transient defects with relatively long lifetime and low excitation energy, such as self-trapped holes, drastically changes the kinetics of energy deposition and type of material modification.
title Controlling ultrafast laser writing in silica glass by pulse temporal contrast
topic Optics
Applied Physics
url https://arxiv.org/abs/2401.09055