High temperature deformation mechanisms in monolithic 3YTZP and 3YTZP containing single wall carbon nanotubes

Fuente: arXiv
Guardado en:
Detalles Bibliográficos
Autores principales: Castillo-Rodríguez, Miguel, Muñoz, Antonio, Domínguez-Rodríguez, Arturo
Formato: Preprint
Publicado: 2024
Materias:
Acceso en línea:
Etiquetas: Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
_version_ 1866929240454201344
author Castillo-Rodríguez, Miguel
Muñoz, Antonio
Domínguez-Rodríguez, Arturo
author_facet Castillo-Rodríguez, Miguel
Muñoz, Antonio
Domínguez-Rodríguez, Arturo
contents Monolithic 3YTZP and 3YTZP containing 2.5 vol.% of single-walled carbon nanotubes (SWCNT) were fabricated by Spark Plasma Sintering (SPS) at 1250 C. Microstructural characterization of the as-fabricated 3YTZP/SWCNTs composite shows a homogeneous CNTs dispersion throughout of ceramic matrix. The specimens have been crept at temperatures between 1100 and 1200 C in order to investigate the influence of the SWCNTs addition on high temperature deformation mechanisms in zirconia. Slightly higher stress exponent values are found for 3YTZP/SWCNTs nanocomposites (n~2.5) compared to monolithic 3YTZP (n~2.0). However, the activation energy in 3YTZP (Q = 715 +- 60 kJ/mol) experiences a reduction of about 25% by the addition of 2.5 vol.% of SWCNTs (Q = 540 +- 40 kJ/mol). Scanning electron microscopy studies indicate that there is no microstructural evolution in crept specimens, and Raman spectroscopy measurements show that SWCNTs preserved their integrity during the creep tests. All these results seem to indicate that the high temperature deformation mechanism is grain boundary sliding (GBS) accommodated by grain-boundary diffusion, which is influenced by yttrium segregation and the presence of SWCNTs at the grain boundary.
format Preprint
id arxiv_https___arxiv_org_abs_2402_06651
institution arXiv
publishDate 2024
record_format arxiv
spellingShingle High temperature deformation mechanisms in monolithic 3YTZP and 3YTZP containing single wall carbon nanotubes
Castillo-Rodríguez, Miguel
Muñoz, Antonio
Domínguez-Rodríguez, Arturo
Materials Science
Monolithic 3YTZP and 3YTZP containing 2.5 vol.% of single-walled carbon nanotubes (SWCNT) were fabricated by Spark Plasma Sintering (SPS) at 1250 C. Microstructural characterization of the as-fabricated 3YTZP/SWCNTs composite shows a homogeneous CNTs dispersion throughout of ceramic matrix. The specimens have been crept at temperatures between 1100 and 1200 C in order to investigate the influence of the SWCNTs addition on high temperature deformation mechanisms in zirconia. Slightly higher stress exponent values are found for 3YTZP/SWCNTs nanocomposites (n~2.5) compared to monolithic 3YTZP (n~2.0). However, the activation energy in 3YTZP (Q = 715 +- 60 kJ/mol) experiences a reduction of about 25% by the addition of 2.5 vol.% of SWCNTs (Q = 540 +- 40 kJ/mol). Scanning electron microscopy studies indicate that there is no microstructural evolution in crept specimens, and Raman spectroscopy measurements show that SWCNTs preserved their integrity during the creep tests. All these results seem to indicate that the high temperature deformation mechanism is grain boundary sliding (GBS) accommodated by grain-boundary diffusion, which is influenced by yttrium segregation and the presence of SWCNTs at the grain boundary.