Comparative study on high temperature mechanical behavior in 3YTZP containing SWCNTs or MWCNTs

Fuente: arXiv
Salvato in:
Dettagli Bibliografici
Autori principali: Castillo-Rodríguez, Miguel, Muñoz, Antonio, Domínguez-Rodríguez, Arturo
Natura: Preprint
Pubblicazione: 2024
Soggetti:
Accesso online:
Tags: Aggiungi Tag
Nessun Tag, puoi essere il primo ad aggiungerne!!
_version_ 1866929241987219456
author Castillo-Rodríguez, Miguel
Muñoz, Antonio
Domínguez-Rodríguez, Arturo
author_facet Castillo-Rodríguez, Miguel
Muñoz, Antonio
Domínguez-Rodríguez, Arturo
contents Effects on mechanical properties of the presence of either single-walled carbon nanotubes (SWCNTs) or multi-walled carbon nanotubes (MWCNTs) in a 3YTZP matrix have been investigated in this work. Thus, monolithic 3YTZP and 3YTZP containing 2.5 vol% either SWCNTs or MWCNTs were fabricated by Spark Plasma Sintering (SPS) at 1250 C. Samples were crept at temperatures between 1100 and 1200 C and stresses between 5 and 230 MPa. Raman spectroscopy measurements indicate the absence of severe damages in the CNTs structure after sintering and testing. Scanning electron microscopy studies show that microstructures do not evolve during creep tests. Mechanical results point out that monolithic 3YTZP exhibits a higher creep resistance than composites since CNTs facilitate grain boundary sliding during high-temperature deformation. SWCNTs and MWCNTs have a similar effect on the high temperature mechanical behavior in 3YTZP where the bundle length and the level of dispersion of CNTs play a crucial role.
format Preprint
id arxiv_https___arxiv_org_abs_2402_08130
institution arXiv
publishDate 2024
record_format arxiv
spellingShingle Comparative study on high temperature mechanical behavior in 3YTZP containing SWCNTs or MWCNTs
Castillo-Rodríguez, Miguel
Muñoz, Antonio
Domínguez-Rodríguez, Arturo
Materials Science
Effects on mechanical properties of the presence of either single-walled carbon nanotubes (SWCNTs) or multi-walled carbon nanotubes (MWCNTs) in a 3YTZP matrix have been investigated in this work. Thus, monolithic 3YTZP and 3YTZP containing 2.5 vol% either SWCNTs or MWCNTs were fabricated by Spark Plasma Sintering (SPS) at 1250 C. Samples were crept at temperatures between 1100 and 1200 C and stresses between 5 and 230 MPa. Raman spectroscopy measurements indicate the absence of severe damages in the CNTs structure after sintering and testing. Scanning electron microscopy studies show that microstructures do not evolve during creep tests. Mechanical results point out that monolithic 3YTZP exhibits a higher creep resistance than composites since CNTs facilitate grain boundary sliding during high-temperature deformation. SWCNTs and MWCNTs have a similar effect on the high temperature mechanical behavior in 3YTZP where the bundle length and the level of dispersion of CNTs play a crucial role.
title Comparative study on high temperature mechanical behavior in 3YTZP containing SWCNTs or MWCNTs
topic Materials Science
url https://arxiv.org/abs/2402.08130