Impact of Annealing Temperature on the Energy Storage Performance of CoO2 Nanoparticles Synthesized via Solid State Reaction

Fuente: arXiv
Saved in:
Bibliographic Details
Main Authors: Akram, Shoaib, Rahman, Muneeb ur, Maula, Fazli, Satti, Osama Tariq, Afzal, Shahbaz, Ali, Fawad
Format: Preprint
Published: 2025
Subjects:
Online Access:
Tags: Add Tag
No Tags, Be the first to tag this record!
_version_ 1866913686047686656
author Akram, Shoaib
Rahman, Muneeb ur
Maula, Fazli
Satti, Osama Tariq
Afzal, Shahbaz
Ali, Fawad
author_facet Akram, Shoaib
Rahman, Muneeb ur
Maula, Fazli
Satti, Osama Tariq
Afzal, Shahbaz
Ali, Fawad
contents The solid-state reaction was used to synthesize CoO2 nanostructured material. Cobalt nitrate tetrahydrate and sodium oxide (NaOH) were combined to produce CoO2 nanostructured material. The three synthesized working electrodes were each tested individually, using 3 M KOH as the electrolyte. The CV analysis of a three-electrode system revealed redox peaks, indicating Faradaic processes. The estimated specific capacitances of CoO2, CoO2 (250oC), CoO2 (300oC) nanostructured material at scan rates of (10) mVs-1 is (223, 348, and 473) Fg-1. The diffraction peaks at 2θ = 26.264o, 33.527o, 37.579, 51.264 and 54.367o correspond respectively to the diffraction planes of 111, 112, 200, 211, and 311 of CoO2 nanostructured material. The annealing temperature, which affects the bandgap, can influence the size, shape, and crystallinity of nanostructures. For the unannealed material, the energy bandgap of CoO2 is 2.00 eV, whereas for the annealed material it ranges from 1.77 to 1.86 eV.
format Preprint
id arxiv_https___arxiv_org_abs_2502_07227
institution arXiv
publishDate 2025
record_format arxiv
spellingShingle Impact of Annealing Temperature on the Energy Storage Performance of CoO2 Nanoparticles Synthesized via Solid State Reaction
Akram, Shoaib
Rahman, Muneeb ur
Maula, Fazli
Satti, Osama Tariq
Afzal, Shahbaz
Ali, Fawad
Materials Science
The solid-state reaction was used to synthesize CoO2 nanostructured material. Cobalt nitrate tetrahydrate and sodium oxide (NaOH) were combined to produce CoO2 nanostructured material. The three synthesized working electrodes were each tested individually, using 3 M KOH as the electrolyte. The CV analysis of a three-electrode system revealed redox peaks, indicating Faradaic processes. The estimated specific capacitances of CoO2, CoO2 (250oC), CoO2 (300oC) nanostructured material at scan rates of (10) mVs-1 is (223, 348, and 473) Fg-1. The diffraction peaks at 2θ = 26.264o, 33.527o, 37.579, 51.264 and 54.367o correspond respectively to the diffraction planes of 111, 112, 200, 211, and 311 of CoO2 nanostructured material. The annealing temperature, which affects the bandgap, can influence the size, shape, and crystallinity of nanostructures. For the unannealed material, the energy bandgap of CoO2 is 2.00 eV, whereas for the annealed material it ranges from 1.77 to 1.86 eV.
title Impact of Annealing Temperature on the Energy Storage Performance of CoO2 Nanoparticles Synthesized via Solid State Reaction
topic Materials Science
url https://arxiv.org/abs/2502.07227