The properties of the nitrogen-vacancy center in milled chemical vapor deposition nanodiamonds

Fuente: arXiv
Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Mameli, Alessandro, Thalassinos, Giannis, Capelli, Marco, Ackermann, Johannes, Mayes, Edwin, Abe, Hiroshi, Ohshima, Takeshi, Luo, Tingpeng, Cimalla, Volker, Knittel, Peter, Gibson, Brant, Jeske, Jan, Dontschuk, Nikolai, Krueger, Anke, Stacey, Alastair, Healey, Alexander, Reineck, Philipp
Format: Preprint
Veröffentlicht: 2025
Schlagworte:
Online-Zugang:
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
_version_ 1866908494704148480
author Mameli, Alessandro
Thalassinos, Giannis
Capelli, Marco
Ackermann, Johannes
Mayes, Edwin
Abe, Hiroshi
Ohshima, Takeshi
Luo, Tingpeng
Cimalla, Volker
Knittel, Peter
Gibson, Brant
Jeske, Jan
Dontschuk, Nikolai
Krueger, Anke
Stacey, Alastair
Healey, Alexander
Reineck, Philipp
author_facet Mameli, Alessandro
Thalassinos, Giannis
Capelli, Marco
Ackermann, Johannes
Mayes, Edwin
Abe, Hiroshi
Ohshima, Takeshi
Luo, Tingpeng
Cimalla, Volker
Knittel, Peter
Gibson, Brant
Jeske, Jan
Dontschuk, Nikolai
Krueger, Anke
Stacey, Alastair
Healey, Alexander
Reineck, Philipp
contents Fluorescent nanodiamonds (FNDs) containing negatively charged nitrogen-vacancy (NV-) centers are vital for many emerging quantum sensing applications from magnetometry to intracellular sensing in biology. However, developing a scalable fabrication method for FNDs hosting color centers with consistent bulk-like photoluminescence (PL) and spin coherence properties remains a highly desired but unrealized goal. Here, we investigate optimized ball milling of single-crystal diamonds produced via chemical vapor deposition (CVD) and containing 2 ppm of substitutional nitrogen and 0.3 ppm of NV- to achieve this goal. The NV charge state, PL lifetime, and spin properties of bulk CVD diamond samples are directly compared to milled CVD FNDs and commercial high-pressure high-temperature (HPHT) FNDs. We find that on average, the relative contribution of the NV- charge state to the total NV PL is lower and the NV PL lifetime is longer in CVD FNDs compared to HPHT FNDs, both likely due to the lower Ns0 concentration in CVD FNDs. The CVD bulk and CVD FNDs on average show similar average T1 spin relaxation times of 3.2 $\pm$ 0.7 ms and 4.7 $\pm$ 1.6 ms, respectively, compared to 0.17 $\pm$ 0.01 ms for commercial HPHT FNDs. Our results demonstrate that ball milling of CVD diamonds enables the large-scale fabrication of NV ensembles in FNDs with bulk-like T1 spin relaxation properties.
format Preprint
id arxiv_https___arxiv_org_abs_2508_13725
institution arXiv
publishDate 2025
record_format arxiv
spellingShingle The properties of the nitrogen-vacancy center in milled chemical vapor deposition nanodiamonds
Mameli, Alessandro
Thalassinos, Giannis
Capelli, Marco
Ackermann, Johannes
Mayes, Edwin
Abe, Hiroshi
Ohshima, Takeshi
Luo, Tingpeng
Cimalla, Volker
Knittel, Peter
Gibson, Brant
Jeske, Jan
Dontschuk, Nikolai
Krueger, Anke
Stacey, Alastair
Healey, Alexander
Reineck, Philipp
Mesoscale and Nanoscale Physics
Materials Science
Fluorescent nanodiamonds (FNDs) containing negatively charged nitrogen-vacancy (NV-) centers are vital for many emerging quantum sensing applications from magnetometry to intracellular sensing in biology. However, developing a scalable fabrication method for FNDs hosting color centers with consistent bulk-like photoluminescence (PL) and spin coherence properties remains a highly desired but unrealized goal. Here, we investigate optimized ball milling of single-crystal diamonds produced via chemical vapor deposition (CVD) and containing 2 ppm of substitutional nitrogen and 0.3 ppm of NV- to achieve this goal. The NV charge state, PL lifetime, and spin properties of bulk CVD diamond samples are directly compared to milled CVD FNDs and commercial high-pressure high-temperature (HPHT) FNDs. We find that on average, the relative contribution of the NV- charge state to the total NV PL is lower and the NV PL lifetime is longer in CVD FNDs compared to HPHT FNDs, both likely due to the lower Ns0 concentration in CVD FNDs. The CVD bulk and CVD FNDs on average show similar average T1 spin relaxation times of 3.2 $\pm$ 0.7 ms and 4.7 $\pm$ 1.6 ms, respectively, compared to 0.17 $\pm$ 0.01 ms for commercial HPHT FNDs. Our results demonstrate that ball milling of CVD diamonds enables the large-scale fabrication of NV ensembles in FNDs with bulk-like T1 spin relaxation properties.
title The properties of the nitrogen-vacancy center in milled chemical vapor deposition nanodiamonds
topic Mesoscale and Nanoscale Physics
Materials Science
url https://arxiv.org/abs/2508.13725