Bromine-methanol etching of semiconductor crystals $Cd_{1-x}Zn_{x}Te_{1-y}Se_{y}$ with different selenium concentrations

Fuente: arXiv
Salvato in:
Dettagli Bibliografici
Autori principali: Naydenov, S. V., Babenko, G. M., Kapustnyk, O. K., Pritula, I. M.
Natura: Preprint
Pubblicazione: 2025
Soggetti:
Accesso online:
Tags: Aggiungi Tag
Nessun Tag, puoi essere il primo ad aggiungerne!!
_version_ 1866914394397474816
author Naydenov, S. V.
Babenko, G. M.
Kapustnyk, O. K.
Pritula, I. M.
author_facet Naydenov, S. V.
Babenko, G. M.
Kapustnyk, O. K.
Pritula, I. M.
contents The effect of the selenium concentration in the composition of the $Cd_{1-x}Zn_{x}Te_{1-y}Se_{y}$ semiconductor crystals on their etching with a bromine-methanol solution was studied. A thermodynamic model is proposed to describe the degree of etching of $Cd_{1-x}Zn_{x}Te$ and $Cd_{1-x}Zn_{x}Te_{1-y}Se_{y}$ crystals. A thermodynamic law is obtained for the first time to describe the change in the etching rate of $Cd_{1-x}Zn_{x}Te_{1-y}Se_{y}$ crystals with different selenium concentrations. Experimental dependencies are constructed for etching trajectories and etching rates with 5% bromine-methanol solutions of $Cd_{1-x}Zn_{x}Te_{1-y}Se_{y}$ crystal samples with nominal $x\sim 0.1$ and selenium concentrations of $y=0$, $y=0.02$, $y=0.06$, and $y=0.1$. The average etching rates were 24${μ}$m/min, 18${μ}$m/min, 15${μ}$m/min, and 13${μ}$m/min. The threshold effect of a strong decrease in the etching rate upon transition from ternary $Cd_{1-x}Zn_{x}Te$ to quaternary $Cd_{1-x}Zn_{x}Te_{1-y}Se_{y}$ crystals, associated with hardening of the crystal structure, is identify and theoretically explained. The obtained experimental data are in good agreement with the theoretical estimates and will be useful for choosing the optimal regimes of crystal treatment.
format Preprint
id arxiv_https___arxiv_org_abs_2509_24532
institution arXiv
publishDate 2025
record_format arxiv
spellingShingle Bromine-methanol etching of semiconductor crystals $Cd_{1-x}Zn_{x}Te_{1-y}Se_{y}$ with different selenium concentrations
Naydenov, S. V.
Babenko, G. M.
Kapustnyk, O. K.
Pritula, I. M.
Materials Science
Applied Physics
Instrumentation and Detectors
The effect of the selenium concentration in the composition of the $Cd_{1-x}Zn_{x}Te_{1-y}Se_{y}$ semiconductor crystals on their etching with a bromine-methanol solution was studied. A thermodynamic model is proposed to describe the degree of etching of $Cd_{1-x}Zn_{x}Te$ and $Cd_{1-x}Zn_{x}Te_{1-y}Se_{y}$ crystals. A thermodynamic law is obtained for the first time to describe the change in the etching rate of $Cd_{1-x}Zn_{x}Te_{1-y}Se_{y}$ crystals with different selenium concentrations. Experimental dependencies are constructed for etching trajectories and etching rates with 5% bromine-methanol solutions of $Cd_{1-x}Zn_{x}Te_{1-y}Se_{y}$ crystal samples with nominal $x\sim 0.1$ and selenium concentrations of $y=0$, $y=0.02$, $y=0.06$, and $y=0.1$. The average etching rates were 24${μ}$m/min, 18${μ}$m/min, 15${μ}$m/min, and 13${μ}$m/min. The threshold effect of a strong decrease in the etching rate upon transition from ternary $Cd_{1-x}Zn_{x}Te$ to quaternary $Cd_{1-x}Zn_{x}Te_{1-y}Se_{y}$ crystals, associated with hardening of the crystal structure, is identify and theoretically explained. The obtained experimental data are in good agreement with the theoretical estimates and will be useful for choosing the optimal regimes of crystal treatment.
title Bromine-methanol etching of semiconductor crystals $Cd_{1-x}Zn_{x}Te_{1-y}Se_{y}$ with different selenium concentrations