Thermodynamic accessibility of Li-Mn-Ti-O cation disordered rock-salt phases
Fuente:
arXiv
Saved in:
| Main Authors: | , , |
|---|---|
| Format: | Preprint |
| Published: |
2026
|
| Subjects: | |
| Online Access: | |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
| _version_ | 1866910190316552192 |
|---|---|
| author | Kam, Ronald L. Wang, Shilong Ceder, Gerbrand |
| author_facet | Kam, Ronald L. Wang, Shilong Ceder, Gerbrand |
| contents | Disordered rock-salt with Li-excess (DRX) cathode phases within the Li-Mn-Ti-O (LMTO) composition space have recently been extensively studied, as they promise to deliver exceptional energy density at low cost in Li-ion batteries. The continued development of LMTO DRX with improved power density and cycling stability requires optimization of the composition and particle size/morphology, which are determined by synthesis conditions such as annealing temperatures and hold times. These challenges motivate our investigation of the phase diagram of the LMTO rock-salt phase space, with a focus on understanding the stability of DRX by quantifying the order-disorder transition temperature ($T_\text{disord}$) as a function of composition. We harness first-principles calculations and X-ray diffraction experiments to establish the LMTO phase diagram, which lies within the LiMnO$_2$ -- Li$_2$MnO$_3$ -- Li$_2$TiO$_3$ pseudo-ternary. Our calculations predict that the LMTO phase diagram at elevated temperature ($700 - 1300$ C) is composed of three phases: DRX, orthorhombic LiMnO$_2$, and layered Li$_2$Mn$_\text{1-y}$Ti$_\text{y}$O$_3$ ($0 < \text{y} < 1$). $T_\text{disord}$ decreases significantly as off-stoichiometry is introduced to the end-point compositions, resulting in a eutectoid phase diagram. Importantly, a significant range of LMTO compositions containing small to moderate fractions of Li-excess and Ti doping (relative to LiMnO$_2$) have $T_\text{disord}$ spanning $700 - 900$ C. These temperatures are substantially lower than conventional DRX synthesis temperatures ($\geq 1000$ C), suggesting the promise of decreasing synthesis temperatures for specific DRX compositions. The compositions containing moderate to high fractions of Mn$^{4+}$ instead have much greater $T_\text{disord}$ and phase separation to layered Li$_2$MnO$_3$ becomes highly favored. |
| format | Preprint |
| id |
arxiv_https___arxiv_org_abs_2603_17263 |
| institution | arXiv |
| publishDate | 2026 |
| record_format | arxiv |
| spellingShingle | Thermodynamic accessibility of Li-Mn-Ti-O cation disordered rock-salt phases Kam, Ronald L. Wang, Shilong Ceder, Gerbrand Materials Science Disordered rock-salt with Li-excess (DRX) cathode phases within the Li-Mn-Ti-O (LMTO) composition space have recently been extensively studied, as they promise to deliver exceptional energy density at low cost in Li-ion batteries. The continued development of LMTO DRX with improved power density and cycling stability requires optimization of the composition and particle size/morphology, which are determined by synthesis conditions such as annealing temperatures and hold times. These challenges motivate our investigation of the phase diagram of the LMTO rock-salt phase space, with a focus on understanding the stability of DRX by quantifying the order-disorder transition temperature ($T_\text{disord}$) as a function of composition. We harness first-principles calculations and X-ray diffraction experiments to establish the LMTO phase diagram, which lies within the LiMnO$_2$ -- Li$_2$MnO$_3$ -- Li$_2$TiO$_3$ pseudo-ternary. Our calculations predict that the LMTO phase diagram at elevated temperature ($700 - 1300$ C) is composed of three phases: DRX, orthorhombic LiMnO$_2$, and layered Li$_2$Mn$_\text{1-y}$Ti$_\text{y}$O$_3$ ($0 < \text{y} < 1$). $T_\text{disord}$ decreases significantly as off-stoichiometry is introduced to the end-point compositions, resulting in a eutectoid phase diagram. Importantly, a significant range of LMTO compositions containing small to moderate fractions of Li-excess and Ti doping (relative to LiMnO$_2$) have $T_\text{disord}$ spanning $700 - 900$ C. These temperatures are substantially lower than conventional DRX synthesis temperatures ($\geq 1000$ C), suggesting the promise of decreasing synthesis temperatures for specific DRX compositions. The compositions containing moderate to high fractions of Mn$^{4+}$ instead have much greater $T_\text{disord}$ and phase separation to layered Li$_2$MnO$_3$ becomes highly favored. |
| title | Thermodynamic accessibility of Li-Mn-Ti-O cation disordered rock-salt phases |
| topic | Materials Science |
| url | https://arxiv.org/abs/2603.17263 |