Effects of compocasting process parameters on microstructural characteristics and tensile properties of A356-SiCp composites

Fuente: arXiv
Saved in:
Bibliographic Details
Main Authors: Khosravi, Hamed, Bakhshi, Hamed, Salahinejad, Erfan
Format: Preprint
Published: 2026
Subjects:
Online Access:
Tags: Add Tag
No Tags, Be the first to tag this record!
_version_ 1866913153984495616
author Khosravi, Hamed
Bakhshi, Hamed
Salahinejad, Erfan
author_facet Khosravi, Hamed
Bakhshi, Hamed
Salahinejad, Erfan
contents The effects of compocasting process parameters on some structural and tensile characteristics of the A356-10% SiCp (volume fraction) composites were studied. Semisolid stirring was carried out at temperatures of 590, 600 and 610 C with stirring speeds of 200, 400 and 600 r/min for 10, 20 and 30 min. The distribution of the SiC particles within the matrix, porosity content and tensile properties of the obtained samples were examined. The structural evaluations show that by increasing the stirring time and decreasing the stirring temperature, the uniformity in the particle distribution is improved; however, by increasing the stirring speed the homogeneity firstly increases and then declines. It is also found that by increasing all of the processing parameters, the porosity content is enhanced. From the tensile characteristics viewpoint, the optimum values of the speed, temperature and time are found to be 400 r/min, 590 C and 30 min, respectively. The contribution of the reinforcement distribution uniformity prevails over that of the porosity level to the tensile properties.
format Preprint
id arxiv_https___arxiv_org_abs_2605_22881
institution arXiv
publishDate 2026
record_format arxiv
spellingShingle Effects of compocasting process parameters on microstructural characteristics and tensile properties of A356-SiCp composites
Khosravi, Hamed
Bakhshi, Hamed
Salahinejad, Erfan
Materials Science
Applied Physics
The effects of compocasting process parameters on some structural and tensile characteristics of the A356-10% SiCp (volume fraction) composites were studied. Semisolid stirring was carried out at temperatures of 590, 600 and 610 C with stirring speeds of 200, 400 and 600 r/min for 10, 20 and 30 min. The distribution of the SiC particles within the matrix, porosity content and tensile properties of the obtained samples were examined. The structural evaluations show that by increasing the stirring time and decreasing the stirring temperature, the uniformity in the particle distribution is improved; however, by increasing the stirring speed the homogeneity firstly increases and then declines. It is also found that by increasing all of the processing parameters, the porosity content is enhanced. From the tensile characteristics viewpoint, the optimum values of the speed, temperature and time are found to be 400 r/min, 590 C and 30 min, respectively. The contribution of the reinforcement distribution uniformity prevails over that of the porosity level to the tensile properties.